A film tear during production and a leak found after packing are different observations. Before changing the film grade or machine settings, identify where the problem appears, when it starts and what changed beforehand.
Use the checks below to build a clearer trial record. They are starting points for investigation, not proof that the film, formulation or machine is responsible.
1、Identify the defect before adjusting the process
Is the film tearing before forming, splitting in a formed cavity, or opening at the seal? Does the leak appear immediately after filling, after packing or during storage?
Photograph the defect and record its position. Keep affected samples and clearly identified comparison samples from the same trial. A repeated location is useful evidence, but it does not establish the cause on its own.
2、Review storage and exposure
PVA water-soluble film responds to moisture in the surrounding air. Check the film grade, batch number, delivery condition, storage history and the time since the protective wrapping was opened.
Follow the storage and conditioning instructions supplied for that specific grade. Do not assume that another supplier's temperature, humidity or conditioning recommendations apply to your film. Protect unused rolls as instructed and record actual conditions where possible.
3、Inspect the film path and roll condition
With the machine safely stopped and following its inspection procedure, check roll alignment, visible edge damage, guides and contact surfaces. Record where the tear begins and whether it occurs at the same point in the film path.
Have the responsible technician check unwinding and tension control against the approved setup. Avoid increasing tension simply to make the web look smoother; a visual improvement alone does not confirm that the operating condition is suitable.
4、Check forming against the approved setup
For a forming process, record the cavity design, film specification, line speed and the settings relevant to that machine. Note whether the defect is at a corner, along a wall or across several cavities.
Confirm that the film grade is intended for the process. Ask the technical team to review the approved operating range before changing settings. There is no single forming temperature or tension setting that can be recommended for every film and machine combination.
Film forming and mould cavities in an empty-pack demonstration. Check suitability through trials with your formulation and equipment.
5、Examine filling and sealing together
Check whether product is reaching the sealing area, whether the films are correctly aligned and whether the seal is continuous. Record the fill amount and the sealing method used.
Film grades and machines can use different sealing methods. Relevant checks may include contact condition, pressure, timing, temperature or wetting control, depending on the actual process. Use the applicable machine and film instructions rather than copying settings from another line.
A seal that looks intact should still be assessed using the agreed package integrity test.
6、Investigate leaks that appear later
If packs pass the initial check but leak later, record the elapsed time, storage conditions and outer packaging used. Keep the formulation version and film batch traceable.
Delayed leakage alone does not prove a compatibility problem. Review film–formulation compatibility, seal integrity and storage or handling conditions together. Agree the trial conditions and acceptance criteria with the technical team before evaluating an alternative film or formulation.
7、Change one variable at a time
Start from a documented baseline and change one approved variable per comparison. Keep the other relevant conditions as consistent as practical.
Record what changed, the number of packs inspected, the number showing defects and when they were checked. Use the same inspection method for each comparison. A short trial can guide the next check; it does not establish long-term storage performance.
8、Prepare a useful troubleshooting record
Before requesting technical review, collect:
- Film grade, batch, thickness and roll dimensions.
- Machine model and the process stage where the defect appears.
- Photographs or a short video showing the defect and its location.
- Formulation reference, fill amount and recent process changes.
- Storage and exposure history, with temperature and humidity records if available.
- Trial settings, inspection method, sample counts and results.
Troubleshooting record checklist
Keep a separate record for the baseline run and the comparison run, using the same fields below.
• Date, time and operator.
• Film grade, batch, thickness and roll size.
• Machine, cavity or lane, and process stage.
• Formulation reference and fill amount.
• Storage conditions and time since unwrapping.
• Defect observed: tear, cavity split or seal opening.
• Defect location and when it was first observed.
• Single approved variable changed: record “No change” for the baseline run and identify the change for the comparison run.
• Machine settings and actual temperature and humidity, if measured.
• Inspection method and time elapsed after production.
• Number of packs inspected and number with defects.
• Photograph or video reference.
• Result and next check agreed with the technical team.
Use this blank record for each comparison. Enter observations rather than a presumed cause. Mark unavailable information as “not recorded”.
Count each defective pack once in the total, even if it has more than one defect; describe individual defects separately. Compare results collected with the same inspection method and timing. Do not send confidential formulation details through a public form; use a formulation reference for the initial review.
For a related checklist, read our
guide to storing PVA water-soluble film. If you need help reviewing the trial, share these records with the ZESONPACK technical team through our contact page. The next step should follow the evidence from your film, formulation and equipment combination.